This tester is used to measure the creep buildup by applying static load to plastic test specimens.By choosing the Chuck, the tester is compatible with conducting tensile tests, condensation tests, and bending tests. The tester can also be assorted with test functions such as relaxation tests, heat shrinkage tests, and thermal impulse tests.
JIS-K7115, ASTM-02990, IS0-899-1
Product Description
-
- No.145-A (PULLEY TYPE)
- No.145-B (BALANCE TYPE)
- No.145-SV (SERVO MOTOR TYPE)
Specification
No.145-A (PULLEY TYPE)
No.145-B (BALANCE TYPE)
| Model | No.145-A | No.145-B |
| Hangings | 3 Hangings, 6 Hangings, 10 Hangings (3 kinds) | |
| Specimen | See JIS-K7162 for reference | |
| Load Method | Pulley Wheel Type | BalancCe Scale Type |
| Test Load | Max. 500 N (50 kgf) | Max. 5 kN (500 kgf) |
| Temperature Range | Max. 200 ·c | |
| Software | Windows Compatible | |
No.145-SV (SERVO MOTOR TYPE)
| Model | 145-SV |
| Hangings | 3 Hangings, 6 Hangings, 10 Hangings (3 kinds) |
| Specimen | See JIS-1<7162 or JIS-K6263 for reference |
| Load Method | Servomotor Type |
| Test Load | Max. 5 kN (500 kgf) |
| Load Detection | Load Cell |
| Displacement | Potentionmeter: Scale 0.1 mm, Stroke o to Max. 300 mm |
| Measurement | Differential Transformer: 0.01 mm, Stroke o to Max. ± 40 mm |
| Temperature Range | Max. 200 ·c |
| Software | Windows Compatible |